Tamil Serial actress & TV Anchor deepa venkat picture gallary. Deepa venkat hot pics, photos, pictures, images, videos, tamil serial actress deepa venkat hot gallery, tamil tv actress deepa venkat, deepa venkat mms scandal, deepa venkat serial actress, deepa venkat latest stills, photo gallery, wallpapers, posters, Vaadagai Veedu Serial In Kalignar TV Press Meet StillsPlease Click The Photo For Clear. Deepa Venkat is a Tamil film and television actress. She is also a popular dubbing artist and a radio disc jockey with Hello FM Chennai. She has played leading roles in over 70 television serials and a few Tamil movies. Tamil actress deepa venkat.
ASTM E8 Metal Tensile Testing ASTM E8 describes tensile testing of metals such as steel or metal alloys. This test determines important mechanical properties such as yield strength, ultimate tensile strength, elongation, and reduction of area. E8 tensile tests determine the ductility and strength of various metals when the materials undergo uniaxial tensile stresses.
Such information is important for alloy development, design, quality control, and comparison of different sets of metals. An electro-mechanical or hydraulic universal testing machine equipped with the appropriate specimen grips, an extensometer and software capable of strain rate control and recording stress – strain data is necessary to conduct this test.
If you need to conduct tensile tests according to ASTM E8, please read the entire specification from the relevant ASTM publication. ASTM E8 Metal Tensile Testing • Measure and record the specimen dimensions necessary to determine the cross sectional area at its smallest point. The original cross sectional area is used for all engineering stress calculations. • Use ink and a scribe or punch to place gage marks on the test specimen at the appropriate gage length.
The distance between the gage marks after the specimen is broken is used to determine the percent elongation at break. Note: To accurately compare elongation values between tests, the gage lengths must be the same. • Zero the testing machine without the specimen inserted in the grips. Then install the specimen in the grips and start loading the sample.
ASTM E8/E8M: Standard Test Methods for Tension Testing of Metallic Materials. $69.00 Print. In Stock Need it fast? Ask for rush delivery. In either paper format or pdf download. Starting in 2008, this standard has been the integrated edition for the and (both of which were withdrawn at that time.) The standard is a collection of test methods that cover the tension testing of metallic materials.
The speed of testing is generally specified in one of three manners: a) the rate of straining of the specimen; b) the rate of stressing of the specimen; or c) the rate of separation of the crossheads. In addition, the test rate is to remain constant through yield but can then be increased when determining ultimate tensile strength and elongation at break. See the ASTM E8 specification for more details. • Run the test until specimen failure or fracture. Remove the broken sample from the machine and fit the fractured ends together.